DescriptionStress corrosion cracking revealed by magnetic particles.JPG
English: A close-up view of the surface of a pipeline showing indications of w:stress corrosion cracking (two clusters of small black lines), as revealed by w:magnetic particle inspection (MPI). The surface was prepared with white contrast paint, and magnetic particles in a liquid suspension were sprayed onto the surface while it was magnetized. Cracks which would normally have been invisible are detectable due to the magnetic particles clustering at the crack openings. The scale at the bottom of the picture is in millimetres. Markings on the pipe were made by a technician for position reference.
La personne qui a associé une œuvre avec cet acte l’a placée dans le domaine public en renonçant mondialement à tous ses droits sur cette œuvre en vertu des lois relatives au droit d’auteur, ainsi qu’à tous les droits juridiques connexes et voisins qu’elle possédait sur l’œuvre, sans autre limite que celles imposées par la loi. Vous pouvez copier, modifier, distribuer et utiliser cette œuvre, y compris à des fins commerciales, sans qu’il soit nécessaire d’en demander la permission.
http://creativecommons.org/publicdomain/zero/1.0/deed.enCC0Creative Commons Zero, Public Domain Dedicationfalsefalse
Légendes
Surface en acier présentant des fissures de corrosion sous contrainte. Deux groupes de petites lignes noires ont été rendus visibles grâce à un traitement préalable avec des particules magnétiques s'accumulant aux lèvres des fissures. Echelle en cm.
View of the surface of a pipeline showing indications of stress corrosion cracking (two clusters of small black lines)
{{Information |Description = A close-up view of the surface of a pipeline showing indications of stress corrosion cracking, as revealed by magnetic particle inspection (MPI). The surface was prepared with white contrast paint, and magnetic par...